ArticleName |
Protective and decorative treatment of low-carbon steels |
ArticleAuthorData |
D. Mendeleev University of Chemical Technology of Russia (Moscow, Russia):
A. A. Abrashov, Cand. Eng., Associate Prof., Dept. of Innovation Materials and Corrosion Protection, e-mail: ngrig108@mail.ru N. S. Grigoryan, Dr. Chem., Prof., Dept. of Innovation Materials and Corrosion Protection, e-mail: vetolmyan@gmail.com Ya. V. Tolmachev, Student, Dept. of Innovation Materials and Corrosion Protection, e-mail: asnis@mail.ru N. A. Asnis, Cand. Tech., Leading Engineer, Dept. of Innovation Materials and Corrosion Protection |
Abstract |
A solution containing 8–12 g/l (NH4)6Mo7O24, 4–12 g/l Na2B4O7·5H2O, 1–2,5 g/l (NH2OH)2·H2SO4 and 3,5-4,5 g/l (NH2)2CO was developed. Аt pH = 5.0–7.0 and at a temperature of 85 °C it allows for 10 minutes to form protective-decorative black coatings on the surface of low-carbon steels that are not inferior in protective ability and decorativeness to coatings obtained from a standard alkaline solution of black oxidation. Solutions containing ammonium heptamolybdate (NH4)6Mo7O24 as the main component and sodium persulfate Na2S2O8 (solution 1) or sodium tetraborate Na2B4O7·5H2O (solution 2) as oxidants were studied. It has been established that high-quality black coatings are obtained in the concentration range of 12–20 g/l (NH4)6Mo7O24; 12–20 g/l Na2S2O8 (solution 1) and 8–12 g/l (NH4)6Mo7O24; 4–12 g/l Na2B4O7·5H2O (solution 2). However, the protective ability of the formed coatings was low, it was determined by the drip express method and was 12–14 s. In order to improve the protective characteristics of the coating, zinc, aluminum, magnesium, or calcium ions were introduced into the solutions. The introduction of zinc or aluminum ions into solutions in an amount of 2.5–3.5 g/l leads to an increase in protective ability by about one and a half to two times. A positive effect on the protective ability of coatings from the introduction of calcium and magnesium ions was not observed. A negative consequence of the introduction of these ions into the solutions was a partial loss of the black color of the coatings, the color depth decreased from 10 to 8 points (with the introduction of Zn2+ and Al3+ ions) and to 9 points (with the introduction of Ca2+ and Mg2+ ions). It was found that the introduction of 1.0–2.5 g/l hydroxylamine into solutions led to a substantial increase in the protective ability of coatings: the protective ability of coatings formed in solution 1 increased from 12–14 to 100 s, and in solution 2, it increased to 300 s. As for urea, it did not affect the protective ability of the coatings, but it allowed to lower the temperature of solution 2 from 98 to 85 °C when it was contained in the solution at a concentration of 3.5–4.5 g/l. The protective ability of the coatings does not change much, and the quality and color of the oxide layers do not deteriorate. The work was carried out with the financial support of the D. Mendeleev UCTR. Project number X-2020-028. |
References |
1. Fattah-alhosseini A., Yazdani Khan H., Heidarpour A. Comparison of Anti-Corrosive Properties between Hot Alkaline Nitrate Blackening and Hydrothermal Blackening Routes. Journal Alloy. Compd. 2016. Vol. 676. pp. 474–480. 2. Eckl M., Zaubitzer S., Köntje C., Farkas A., Kibler L.A., Jacob, T. An Electrochemical Route for Hot Alkaline Blackening of Steel: A Nitrite Free Approach. Surfaces. 2019. Vol. 2, Iss. 2. pp. 216–228. 3. Abrashov А. А., Grigoryan N. S., Vagramyan Т. А., Mardashova Ya. А., Statsyuk V. N. et. al. Low temperature black phosphating process. Galvanotekhnika i obrabotka poverkhnosti. 2015. Vol. 23. No. 4. pp. 38–42. 4. Kusmierczak S., Makovský M. Problems of Blackening of Steel Parts in Technical Practice. MATEC Web Conf. 2018. 244. 01012. 5. Yufeng Zhang, Xi Zhang, Minrui Li et al. Study of Film Layer Structure and Resistance on High Strength Room Temperature Blackening. Applied Mechanics and Materials. 2014. Vol. 687–691. pp. 4183–4186. 6. Orlov D. N., Vershok D. B., Gorodetsky А. Е., Kuznetsov Yu. I., Vagramyan Т. А. Modification of magnetite coatings formed on steel in nitrate solutions. Korroziya: materialy, zashchita. 2015. No. 4. pp. 31–36. 7. Vershok D. B., Kuznetsov Y. I., Orlov D. N., Ionov Y. A., Sorokina O. V. Two-step oxidation of steel in nitrate solutions. Protection of Metals and Physical Chemistry of Surfaces. 2016. Vol. 52, Iss. 7. pp. 1166–1169. 8. Vershok D. B., Kuznetsov Yu. I., Zalavutdinov R. Kh. On the possibility of reducing the oxidation temperature of steel in a nitrate solution. Korroziya: materialy, zashchita. 2017. No. 7. pp. 40–44. 9. Abrashov A. A., Grigoryan N. S., Vagramyan T. A., Shcherbina E. A. Durable light absorbing coatings for structural steels. CIS Iron and Steel Review. 2020. Vol. 19. pp. 71–74. 10. Fadeev I. V., Illarionov I. Е., Sadetdinov Sh. V. Aminoborate solution for obtaining magnetite coatings on steel. Vestnik Moskovskogo avtomobilno-dorozhnogo gosudarstvennogo technicheskogo universiteta. 2016. No. 1. pp. 68–74. 11. Frolenkova S. V., Donchenko М. I., Sribnaya О. G., Lisenko О. Yu. Oxide conversion coatings and their protective properties against corrosion of mild steel. Naukovi visri NTUU "KPI". 2009. No. 3. pp. 123–130. 12. Frolenkova S. V., Donchenko М. I., Motronyuk T. I. Passivation of mild steel in sodium tetraborate solution. Voprosy khimii i khimicheskoy tekhnologii. 2011. No. 4. pp. 250–252. 13. Donchenko М. I., Frolenkova S. V., Motronyuk T. I. Mechanism of passivation of carbon steel by oxometallates and halogens in aqueous solutions. Voprosy khimii i khimicheskoy tekhnologii. 2016. No. 2. pp. 26–31. 14. GOST 9.305–84. Unified system of corrosion and ageing protection. Metal and non-metal inorganic coatings. Introduced: 01.01.1986. 15. GOST 9.302–88. Unified system of corrosion and ageing protection. Metal and non-metal inorganic coatings. Control methods. Introduced: 01.01.1990. 16. GOST 9.401–2018. Unified system of corrosion and ageing protection. Paint coatings. General requirements and methods of accelerated tests on resistance to the influence of climatic factors. Introduced: 01.07.2019. 17. ASTM B117–19. Standard Practice Operating Salt Spray (Fog) Apparatus. 11 p. 18. Grubin S. D., Grigoryan N. S., Akimova Е. F., Kharlamov V. I. et. al. Chromate-free passivation of zinc coatings. Galvanotekhnika i obrabotka poverkhnosti. 2003. Vol. 11. No. 2. pp. 35–40. 19. Grubin S. D., Grigoryan N. S., Akimova Е. F., Kharlamov V. I. et. al. Amorphous adhesive phosphate layers with improved barrier properties. Galvanotekhnika i obrabotka poverkhnosti. 2003. Vol. 11. No. 3. pp. 35–41. 20. Lobanov S. А., Poylov V. Z., Sofronova А. V. Purification of waste water from ammonium ions by oxidation. Zhurnal prikladnoy khimii. 2006. Vol. 79. No. 10. pp. 1638–1641. 21. Grigoryan N. S., Abrashov А. А., Vagramyan Т. А., Kostyuk А. G. Passivation of ferrous and non-ferrous metals in solution based on gallic acid esters. Khimiya i tekhnologiya organicheskikh veshchestv. 2017. No. 4. pp. 55–63. 22. Abrashov А. А., Grigoryan N. S., Vagramyan Т. А., Papirov R. V., Styazhkina М. I. Low-temperature crystalline phosphating solutions. Galvanotekhnika i obrabotka poverkhnosti. 2013. Vol. 21. No. 4. pp. 40–45. |