PYROMETALLURGY | |
ArticleName | Processing of technology of ore copper-nickel concentrate roasting at aggregative-laboratory setting of boiling layer |
ArticleAuthor | Portov A. B., Ozerov S. S., Savinova Yu. A., Tsemekhman L. Sh. |
ArticleAuthorData | LLC “Institute “Gipronikel”, Saint Petersburg, Russia: |
Abstract | Technology of partial oxidation roasting of ore copper-nickel concentrate, mixed with silt of technogenic Nyud-Yavr Lake deposit, was carried out on aggregative-laboratory unit of boiling layer. There was studied the influence of various parameters (charge fluid bed furnace capacity; feed rate of blow gas and their oxygen content in layer temperature) on roasting indicators (cinder output, its size and cyclone dust size; content of residual sulfides in this cinder and cyclone dust, structure and material composition of roasting products). There was found that the roasting-formed dust is very fine, its material composition is unstable, and it is non-condition product for subsequent electrical melt. Organization of complete dust recycling is not possible with low-temperature roasting (720–740 oC). At the same time, dust removal is reached by 40–53%, if roasting is carried out at the temperature of 820–840 oC. The maximum extraction of silt into cinder is 95–98%. Increasing of roasting temperature leads to a deeper sulfur removal from cinders and transfer of main part of non-ferrous metals in the deep oxidized (spinel and ferrite) components. There were defined the parameters, which require the process of obtaining of optimal composition roasting products (cinder) in maximum amount. Process adjustment and maintaining at the given parameters is achieved by varying of oxygen content in blow gases and the time of material presence in a fluidized bed (sector gates opening frequency). Feed of concentrate as a slurry sludge injection into the fluid bed furnace through nozzles is possible as well as furnace operation for complete dust removal. However, for the purpose of maintaining of required sulfur content of dust, it is necessary to decrease the roasting temperature of 600–610 oC, leading predominantly to sulfates’ formation in cinder |
keywords | Boiling layer, cinder, dust recycling, ore concentrate, copper-nickel concentrate, technogenic slit, oxidizing roasting |
References | 1. Ezhov E. I., Murashov V. D. et al. Sostoyanie proizvodstva nikelya i kobalta na vedushchikh metallurgicheskikh predpriyatiyakh Kanady (Status of production of nickel and cobalt at leading Canadian metallurgical enterprises). Moscow : TsNIItsvemet, 1989. pp. 70–73. 8. Blatov I. A., Klementev V. V., Portov A. B., Tsemekhman L. Sh. Okislitelnyy obzhig medno-nikelevogo kontsentrata (Oxidizing roasting of copper-nickel concentrate). Tezis doklada II Mezhdunarodnogo simpoziuma “Problemy kompleksnogo ispolzovaniya rud” (Thesis of a report of the II International symposium “Problems of complex use of ores”). Saint Petersburg, May 10–20, 1994. pp. 177–178. |
Language of full-text | russian |