Название |
Features of the formation of niobium-rich carbide phases in the
melt and their effect on the resistance of high-strength casing pipes to sulfide stress corrosion cracking |
Информация об авторе |
Volgograd State Technical University, Volgograd, Russia
L. V. Palatkina, Cand Eng., Associate Prof., Dept. of Materials Technology, e-mail: lv.palatkina@yandex.ru M. V. Matasova, Magister, Dept. of Materials Technology, e-mail: matasova.mary2016@mail.ru M. V. Kirilichev, Head of Laboratory, Dept. of Materials Technology, e-mail: tecmat@vstu.ru
JSC “Volzhsky Pipe Plant“, Volzhsky, Russia
M. Yu. Chubukov, Cand. Eng., Head of the Central Plant Laboratory, e-mail: chubukovmu@vtz.ru |
Реферат |
It is shown that the focus (foci) of metal destruction of corrosion-resistant high-strength casing pipes made of steel type 26KhGMF, when assessing resistance to sulfide stress corrosion cracking (SCR) according to method A of the NACE TM 0177 standard, is located on the surface of the sample and represents a pitting or a corrosion ulcer. For standard samples made of steel type 26KhGMF, a relationship has been established between the morphological features of the macro-relief of fractures and the development of fracture by the SCR mechanism. A sequential change of three main stages of destruction was recorded: I – the stage of brittle corrosion destruction with scars emanating from the fracture site; II – the stage of corrosion cracking with uneven furrowing according to the type of fatigue lines, without signs of plastic deformation of the metal; III – the stage of viscous destruction due to the combined action of plastic deformation (reduction of the cross section of the sample) and corrosion cracking (accumulation of hydrogen in places with high stress localization). In the metal of casing pipes made of steel type 26KhGMF (microalloyed Nb in an amount up to 0.03 % by weight) by the method of color etching in hot sodium picrate, phases such as MeС and Me(C,N) rich in niobium (Nb from 45.05 to 59.71 % by weight) were revealed. The lines (from 5.3 to 22.8 microns in length) consist of inclusions of various dispersities (from 0.3 to 3.8 microns) and shapes (oval, rounded, cubic and block). Based on a comprehensive analysis of the double Fe-Nb state diagram, a quasi-binary section of the eutectic Fe-NB type with a triple Fe-Nb-C system, a pseudobinar diagram of the state of 26KhGMF steel, a sequential change of solidification mechanisms and different solubility of Nb in δ-Fe and γ-Fe (for conditions of equilibrium crystallization of 26KhGMF microalloyed Nb steel in an amount up to 0.03 % by weight by weight) The possibility of formation of niobium-rich carbide and carbonitride phases in the melt is substantiated. The classification of the carbide (carbonitride) phase rich in Nb has also been clarified: primary, micron-sized niobium carbide (NbC)I is formed in the melt before the steel solidifies; secondary, eutectic, micron-sized niobium carbide (NbC)II is formed at the final stage of crystallization of steel as a result of a eutectic reaction; tertiary, nanoscale niobium carbide (NbC)III is isolated from a solid solution of austenite during heat treatment. Increasing the resistance to cracking in a hydrogen sulfide environment for microalloyed Nb steel of type 26KhGMF is possible by eliminating the very component of the nucleation of corrosion cracks and excluding areas of hydrogen accumulation with increased capacity in the metal volume, i.e., provided that the formation of micron-sized Nb-rich carbide and carbonitride phases is prevented. |
Библиографический список |
1. Elkhodbia M., Negi A., Mubarak G., Barsoum I. et al. Review on sulfide stress cracking in sour service for OCTG and recent advances in modeling of hydrogen-assisted fracture. Geoenergy Science and Engineering. 2023. Vol. 230, Iss. 10. 212174. DOI: 10.1016/j.geoen.2023.212174 2. Mohtadi-Bonab M. A. Effects of different parameters on initiation and propagation of stress corrosion cracks in pipeline steels: A review. Metals. 2019. Vol. 9. 590. DOI: 10.3390/met9050590 3. Wang Z., Wang P., Zeng D., Shi T. et al. A study on the influential factors of stress corrosion cracking in C110 casing pipe. Materials. 2022. Vol. 15, Iss. 3. 801. DOI: 10.3390/ma15030801 4. Shiryaev A. G., Chetverikov S. G., Chikalov S. G., Pyshmintsev I. Yu., Krylov P. V. Production technologies of seamless steel pipes for the extraction of hard-to-recover hydrocarbons. Izvestiya vuzov. Chernaya metallurgiya. 2018. Vol. 61. No. 11. pp. 866–875. DOI: 10.17073/0368-0797-2018-11-866-875 5. Uskov D. P. Improving the performance properties of high-strength complex alloy steels for casing pipes in cold-resistant and corrosion-resistant versions: Dissertation ... Candidate of Technical Sciences. Chelyabinsk. 2023. 158 p. 6. Putilova E. A., Zadvorkin S. M., Veselov I. N., Pyshmintsev I. Yu. Investigation of the structure and physico-mechanical properties of promising high-strength economically alloyed steel for oil and gas field pipes operated under extreme conditions. Fizika metallov I metallovedenie. 2021. Vol. 122. No. 9. pp. 993–1000. DOI: 10.31857/S0015323021090114 7. Palatkina L. V., Galagan V. V., Matasova M. V., Chubukov M. Yu. The effect of electromagnetic stirring on processes of alloy crystallization and the macro- and microstructure of continuously cast billets for production of pipes which are resistant to hydrogen sulfide. Chernye metally. 2023. No. 10. pp. 63–69. 8. NACE Standard TM0177-2016. Laboratory testing of metals for resistance to sulfide stress cracking and stress corrosion cracking in H2S environments. Houston, TX: NACE, 2016. 9. GOST 31446–2017. Steel casing and pump-compressor pipes for the oil and gas industry. Introduced: 01.07.2018. 10. STO TMK 56601056-0008-2006. Continuous cast round tube billet for the manufacture of seamless pipes. Technical conditions. The standard of the organization. Chelyabinsk : RosNITI OJSC. 2018. 29 p. 11. Ioffe A. V. The mechanism of destruction of tubular steels in a hydrogen sulfide-containing medium: Abstract of the Dissertation. ... of Candidate of Technical Sciences. Tolyatti 2000. 24 p. 12. Panchenko E. V. et al. Metallographic laboratory: a textbook for universities. Edited by B. G. Livshits. 2nd edition. Moscow : Metallurgy. 1965. 439 p. 13. Shashkova L. V. Fractal-synergetic aspects of micro-damage, destruction and optimization of steel structure under conditions of hydrogen brittleness and hydrogen sulfide corrosion cracking. Orenburg : Publishing and printing complex “Universitet”. 2013. 305 p. 14. Balter M. A., Lyubchenko A. P., Aksenova S. I. Fractography — a remedy for diagnostics of destroyed parts. Moscow : Mashinostroenie. 1987. 159 p. 15. Vinograd M. I. Inclusions in steel and its properties. Moscow : Metallurgizdat. 1963. 252 p. 16. Bannykh O. A. et al. Diagrams of the state of double and multicomponent systems based on iron: a handbook. Moscow : Metallurgiya. 1986. 439 p. 17. Heisterkamp F., Hulka K., Matrosov Yu. I. et al. Niobium containing low-alloy steels. Moscow : Intermet Inzhiniring. 1999. 90 p. 18. Zheng S., Davis C., Strangwood M. Elemental segregation and subsequent precipitation during solidification of continuous cast Nb – V – Ti high-strength low-alloy steels. Materials Characterization. 2014. Vol. 95. pp. 94–104. DOI: 10.1016/j.matchar.2014.06.008 19. Zhang Y., Yang J. Formation of Nb(C,N) carbonitride in cast austenitic heat-resistant steel during directional solidification under different withdraw rates. Materials. 2018. Vol. 11. 2397. DOI: 10.3390/ma11122397 20. Bunin K. P., Malinochka Ya. N., Taran Yu. N. Fundamentals of metallography of cast iron. Moscow : Metallurgiya. 1969. 416 p. 21. Elliott R. Management of eutectic solidification. Moscow : Metallurgiya. 1987. 352 p. 22. Jeglitsch F. Niobium in tool steels and cemented carbides. Proceedings of the International Symposium Niobium. 2001. Bridgeville. TMS. 2001. pp. 1001–1040. 23. DeArdo A. J. Niobium in modern steels. International Materials Reviews. 2003. Vol. 48. pp. 371–402. 24. Wu Lailei, Wang Yachun, Yan Zhigang, Zhang Jingwu et al. The phase stability and mechanical properties of Nb–C system: Using first-principles calculations and nano-indentation. Journal of Alloys and Compounds. 2013. Vol. 561. pp. 220–227. DOI: 10.1016/j.jallcom.2013.01.200 25. Shishlonova, A. N., Adishchev P. G., Malkov M. V. Input control of ferroniobium intended for microalloying steel. Vestnik Magnitogorskogo gosudarstvennogo tekhnicheskogo universiteta im G. I. Nosova. 2021. Vol. 19. No. 1. pp. 69–74. DOI: 10.18503/1995-2732-2021-19-1-69-74 26. Korchemkina N. V. Physico-chemical properties of iron-niobium, iron-niobium-silicon and ironniobium-aluminum alloys: abstract of the dissertation of the Candidate of Chemical Sciences. Institute of Metallurgy of the Ural Branch of the Russian Academy of Sciences. Ekaterinburg, 2006. 22 p. 27. Shaskolskaya M. P. Crystallography: a textbook. Manual for higher education institutions. 2nd edition. Moscow : Vysshaya shkola. 1984. 376 p. 28. Zeng T., Zhang Shuzhan, Shi Xianbo, Wang Wei et al. Effects of the primary NbC elimination on the SSCC resistance of a HSLA steel for oil country tubular goods. Materials. 2021. Vol. 14. 5301. DOI: 10.3390/ma14185301 29. Tian Y., Zhao MC., Zeng YP. et al. Elimination of primary NbC carbides in HSLA steels for oil industry tubular goods. JOM. 2022. Vol. 74. pp. 2409–2419. DOI: 10.1007/s11837-022-05202-6 30. Song Eun Ju. Hydrogen desorption in steels. Thesis for doctor of philosophy. computational metallurgy. Graduate Institute of Ferrous Technology Pohang University of Science and Technology. 2015. 106 p. 31. Kondratiev S. Yu., Svyatysheva E. V., Anastasiadi G. P., Danilova M. A. Features of the formation of the structure of niobium carbide in cast heat-resistant alloys based on the Fe-Cr-Ni system. Nauchno-tekhnicheskie vedomosti Sankt-Peterburgskogo politekhnicheskogo universiteta. 2016. No. 4 (254). pp. 191-209. |