Название Effect of the chemical composition of aluminium alloys on the structure and properties of micro-arc oxidation coatings
DOI 10.17580/tsm.2023.11.08
Автор Dudareva N. Yu., Kolomeychenko A. V., Deev V. B., Zaynullina L. I.
Информация об авторе

Ufa University of Science and Technology, Ufa, Russia

N. Yu. Dudareva, Professor at the Department of Internal Combustion Engines, Chief Researcher, Doctor of Technical Sciences, Associate Professor, e-mail: dudareva.nyu@ugatu.su

L. I. Zaynullina, Associate Professor of the Department of Materials Science and Physics of Metals, Junior Researcher, Candidate of Technical Sciences, e-mail: Zaynullina.LI@yandex.ru

 

Central Scientific Research Automobile and Automotive Engines Institute NAMI, Moscow, Russia
A. V. Kolomeychenko, Head of the Innovative Technology Department, Centre for Agricultural Engineering, Doctor of Technical Sciences, Professor, e-mail: a.kolomiychenko@nami.ru

 

Wuhan Textile University, Wuhan, China1Vladimir State University named after Alexander and Nikolay Stoletovs, Vladimir, Russia2 ; National University of Science and Technology MISiS, Moscow, Russia3
V. B. Deev, Professor at the Faculty of Mechanical Engineering and Automation1, Chief Researcher2, Professor at the Department of Metal Forming3, Doctor of Technical Sciences, Professor (Соrresponding Autor), e-mail: deev.vb@mail.ru

Реферат

This paper looked at the effect of the chemical composition of aluminium alloys on the structure and properties of coatings formed by micro-arc oxidation. Thus, the thickness of the formed layer, as well as its porosity and corrosion resistance were determined. Specimens of aluminium alloys with different concentrations of silicon were used for all studies: a hypoeutectic alloy AK4-1 with Si 0.4% and a foreign-made hypereutectic alloy M244 with Si 26%. Micro-arc oxidation was performed in the same mode in a silicatealkaline electrolyte in a capacitor unit for 2 hours. SEM images were used for a structural study of the resulting coatings. The porosity of the coatings was determined by image processing in ImageJ. The corrosion resistance of the specimens was analyzed based on the mass rate of corrosion. For this, the specimens were submerged in a corrosive solution. Analysis of the obtained results showed that the silicon in the aluminium alloy causes a high poro sity of the coatings formed. Silicon was found to influence the behaviour of the electric parameters of the process by bringing up the anode current value while not affecting the thickness of the coating. Analysis of the photographs of microsections showed that the layer formed on AK4-1 alloy has higher density and low porosity, but it also has through cracks. Irrespective of porosity, the corrosion resistance of coated specimens is almost the same. Due to the presence of such layer, the corrosion resistance of the AK4-1 specimens increased by 1.72 times, whereas for the M244 specimens it is 1.2 times lower.

This research was funded under Governmental Assignment No. FEUE-2023-0007 (UUST) by the Ministry of Science and Higher Education of the Russian Federation.

Ключевые слова Micro-arc oxidation, aluminum alloys, microstructure, coating, porosity, thickness, corrosion resistance
Библиографический список

1. Ayatollahi M. R., Mohammadi F., Chamani H. R. Thermo-mechanical fatigue life assessment of a diesel engine piston. International Journal of Automotive Engineering. 2011. Vol. 1, No. 4. pp. 256–266.
2. Caldera M., Massone J. M., Martínez R. A. Failure analysis of a damaged direct injection diesel engine piston. Journal of Failure Analysis and Prevention. 2017. No. 17. pp. 979–988. DOI: 10.1007/s11668-017-0327-y
3. Makarov A. R., Smirnov S. V., Osokin S. V., Pyatov I. S. et al. Structural materials for internal combustion engine pistons. Izvestiya MGTU “MAMI”. 2013. No. 1. pp. 118–125.
4. Myagkov L. L., Mahkamov K., Chainov N. D., Makhkamova I. et al. Conventional and advanced internal combustion engine materials. Alternative Fuels and Advanced Vehicle Technologies for Improved Environmental Performance (Second Edition). Woodhead Publishing. 2022. pp. 353–412. DOI: 10.1016/B978-0-323-90979-2.00008-1
5. Kissell J. R., Pantelakis S. G., Haidemenopoulos G. N. Aluminum and aluminum alloys. Handbook of Advanced Materials: Enabling New Designs. 2004. pp. 321–463. DOI: 10.1002/0471465186.ch9
6. Grigorieva I. O., Dresvyannikov A. F. Anodic behaviour of aluminium in neutral electrolytes. Bulleten Kazanskogo Tekhnologicheskogo Universiteta. 2010. No. 7. pp. 153–161.
7. Suminov I. V., Epelfeld A. V., Lyudin V. B. et al. Micro-arc oxidation: Theory, technology, equipment. Moscow : EKOMET, 2005. 368 p.
8. Shandarov B. V., Morozov E. M., Zhukovskiy A. V. Fundamentals of micro-arc oxidation: Learner’s guide. Moscow : ID “Alyans”, 2008. 80 p.
9. Malyshev V. N., Gantimirov B. M., Volkhin A. M., Kim S. L. Raising the anti-friction properties of wear-resistant MAO coatings. Chemical Physics and Mesoscopy. 2013. Vol. 15, No. 2. pp. 285–291.
10. Dudareva N. Yu., Kolomeichenko A. V., Deev V. B., Sitdikov V. M. Porosity of oxide ceramic coatings formed by micro-arc oxidation on high-silicon aluminum alloys. Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques. 2022. Vol. 16, No. 6. pp. 1308–1314. DOI: 10.1134/S1027451022060362
11. Trushkina T. V., Mikheev A. E., Girn A. V. Corrosion resistance of MAO coatings in corrosive environments. Vestnik SibGAU. 2014. No. 1. pp. 179–184.
12. Kolomeichenko A. V., Chernyshov N. S., Titov N. V., Logachev V. N. Investigation of corrosion resistance of aluminum alloy products with protective coatings formed by plasma electrolytic oxidation. Surface Engineering and Applied Electrochemistry. 2017. Vol. 53, No. 4. pp. 322–326. DOI: 10.3103/S1068375517040081
13. Dudareva N. Y., Ivashin P. V., Gallyamova R. F., Tverdokhlebov A. Y. et al. Structure and thermophysical properties of oxide layer formed by microarc oxidation on AK12D Al – Si alloy. Metal Science and Heat Treatment. 2021. Vol. 62. pp. 701–708. DOI: 10.1007/s11041-021-00625-5
14. Curran J. A., Kalkanci H., Magurova Yu., Clyne T. W. Mullite-rich plasma electrolytic oxide coatings for thermal barrier applications. Surface and Coatings Technology. 2007. Vol. 201. pp. 8683–8687. DOI: 10.1016/j.surfcoat.2006.06.050
15. Liu Y. J., Xu J. Y., Lin W., Gao C. et al. Effects of different electrolyte systems on the formation of micro-arc oxidation ceramic coatings of 6061 aluminum alloy. Reviews on Advanced Materials Science. 2013. Vol. 33. pp. 126–130.
16. Orlova D. V., Trushkina T. V., Vakhteev E. V., Alyakretskiy R. V. Examining the porosity of oxide coatings on aluminium alloys. Trudy MAI. 2013. Iss. 68. pp. 1–7.
17. Curran J. A., Clyne T. W. Porosity in plasma electrolytic oxide coa tings. Acta Materialia. 2006. No. 54. pp. 1985–1993. DOI: 10.1016/j.actamat.2005.12.029
18. Ivashin P. V., Krishtal M. M., Tverdokhlebov A. Ya., Polunin A. V. et al. Different-size porosity and heat conductivity of oxide layers formed by plasma electrolytic oxidation on AK12D silumin. Frontier Materials & Technologies. 2022. No. 4. pp. 49–69. DOI: 10.18323/2782-4039-2022-4-49-69
19. Pistons and engine testing. MAHLE Int. GmbH. Springer Fachmedien Wiesbaden, 2016. 295 p. DOI: 10.1007/978-3-658-09941-1
20. GOST 4784–97. Aluminium and wrought aluminium alloys. Grades. Introduced: 01.07.2000.
21. ImageJ. Research Services Branch of the National Institute of Mental Health. 1997. Available at: https://imagej.nih.gov/ij/
22. GOST 9.904–82. Unified system of corrosion and ageing protection. Alluminium alloys. Accelerated test method for exfoliating corrosion. Introduced: 01.07.1983.
23. Yerokhin A. L., Snizhko L. O., Gurevina N. L., Leyland A. et al. Spatial characteristics of discharge phenomena in plasma electrolytic oxidation of aluminium alloy. Surface and Coatings Technology. 2004. Vol. 177-178. pp. 779–783. DOI: 10.1016/j.surfcoat.2003.06.020
24. Mikheev A. E., Girn A. V., Vakhteev E. V., Alekseeva E. G. et al. Forming of the structure and composition of MAO coatings on aluminium alloys. Vestnik SibGAU. 2012. No. 2/48. pp. 206–212.

Language of full-text русский
Полный текст статьи Получить
Назад