Журналы →  CIS Iron and Steel Review →  2021 →  №1 →  Назад

Metal Science and Metallography
Название Metallography of non-metallic inclusions in pipe metal and impact assessment of defect structures on non-destructive testing outcomes
DOI 10.17580/cisisr.2021.01.10
Автор D. V. Zhukov, S. V. Konovalov, A. A. Melnikov, Danhe Chen
Информация об авторе

Nanjing University of Science and Technology (Nanjing, China)1 ; Gazprom Transgaz Samara LLC (Samara, Russia)2:

D. V. Zhukov1,2, Head of the Database Maintenance Group of the Equipment and Facilities Diagnostics Service, Post Graduate of Samara National Research University, e-mail: dzetlab@yandex.ru

 

Nanjing University of Science and Technology (Nanjing, China):
S. V. Konovalov*, Dr. Eng., Prof., Head of Dept. of Materials Technology and Aviation Material Science, e-mail: ksv@ssau.ru

Danhe Chen, Dr. Eng., Prof., School of Mechanical Engineering, e-mail: juliachen@njust.edu.cn

 

Samara National Research University (Samara, Russia):
A. A. Melnikov, Cand. Eng., Associate Prof., Dept. of Materials Technology and Aviation Material Science, e-mail: melnickov.alex@yandex.ru

*Corresponding author: S. V. Konovalov, Dr. Eng., Prof.

Реферат

Low carbon steel pipes represent a core component in the gas pipeline system, so it is necessary to improve constantly diagnostic operations and assessment methods of their technical state. Studies on objects operated in diverse conditions within a long period provide reliable data on the real behavior of materials. A key issue is the investigation of characteristics and behavior of products with primarily incorporated defective structures undetected while manufacturing and constructing. It is difficult to forecast the behavior of such defects, in addition, considerably more work need to be done to determine their development, detection methods, and more importantly, their hazards. The reported study investigates the phases, structure and sizes of inclusions detected in the defective pipe metal in the natural gas pipeline. The property that characterizes defects of interest is their concentration within one pipe section in combination with diverse thickness, composition, and location in the pipe wall. Defects are found at various depths, forming one, two and more layers. The difference in structure and phase composition is outlined. The research has pointed out principal inclusions represent fragments of charge materials — fluorite and broken fireclay brick, a number of defects result from casting defects, e.g. gas bubbles and shrinkage holes. Non-destructive ultrasonic testing is implemented; the importance of thickness and structure of inclusions for measurement data has been realized.

Ключевые слова Inclusions, lamination, metallurgical defect, ultrasonic thickness measurement, natural gas pipeline
Библиографический список

1. European gas pipeline incident data group https://www.egig.eu/startpagina (accessed 20.03.2020).
2. About Gazprom. http://www.gazprom.ru/about/ (accessed 20.03.2020).
3. Harionovskij V.V. Reliability of main natural gas pipelines: rise, development, and present day state. Gazovaya promyshlennost. 2019. No. 1. pp. 56–68.
4. Maruschak P., Danyliuk I., Prentkovskis O., Bishchak R., Pylypenko A., Sorochak A., Degradation of the main gas pipeline material and mechanisms of its fracture. Journal of Civil Engineering and Management. 2014. Vol. 20. pp. 864–872. DOI: 10.3846/13923730.2014.971128
5. Bolshakov A. M., Syromyatnikova A. S. Degradation of mechanical properties and structure-phase state of pipe metal in main gas lines under long-term operation in Northern regions. Prirodnye resursy Arktiki i Subarktiki. 2018. Vol. 23 (1). pp. 75–80.
6. Hutsaylyuk V., Maruschak P., Konovalenko I., Panin S., Bishchak R., Chausov M., Mechanical properties of gas main steels after long-term operation and peculiarities of their fracture surface morphology. Materials. 2019. Vol. 12 (3). p. 491. DOI: 10.3390/ma12030491
7. Marvin C. W. Determining the strength of corroded pipe. Materials protection and Performance. 1972. No. 11. pp. 34–40.
8. Al-Owaisi S. S., Becker A. A., Sun W. Analysis of shape and location effects of closely spaced metal loss defects in pressurised pipes. Engineering Failure Analysis. 2016. Vol. 68. pp. 172–186. DOI: 10.1016/j.engfailanal.2016.04.032
9. Veliyulin I. I. Determination of allowable parameters in corroded pipes. Territoriya Neftegaz. 2019. No. 11. pp. 40–47.
10. Afanasyev A. V., Melnikov A. A., Konovalov S. V., Vaskov M. I. The analysis of the influence of various factors on the development of stress corrosion defects in the main gas pipeline walls in the conditions of the European part of the Russian Federation. International Journal of Corrosion. 2018. 1258379. DOI: 10.1155/2018/1258379
11. Afanasyev A. V., Melnikov A. A., Savin D. V., Zhukov D. V., Vaskov M. I. A possibility to assess visually the depth of stress-corrosion defects in pipe walls of direct natural gas lines. Polzunovsky vestnik. 2018. No. 4. pp. 170–175. DOI: 10.25712/ASTU.2072-8921.2018.04.034
12. Panagopoulos C., Georgiou E., Giannakopoulos K., Orfanos P. Effect of pH on stress corrosion cracking of 6082 Al alloy. Metals. 2018. No. 8. p. 578. DOI: 10.3390/met8080578
13. Pinheiro B., Pasqualino I., Cunha S. Stress concentration factors of dented pipelines. Proceedings of IPC2006 6th International Pipeline Conference. Calgary. 2006. pp. 335–344. DOI: 10.1115/IPC2006-10598
14. Palmer-Jones R., Turner S., Hopkins P. A Proposal for the development of an international recommended. Practice in pipeline defect assessment and repair selection. International Conference on The Evaluation and Rehabilitation of Pipelines. Prague. 2008. pp. 1–27.
15. Vilkys T., Rudzinskas V., Prentkovskis O., Tretjakovas J., Višniakov N., Maruschak P. Evaluation of failure pressure for gas pipelines with combined defects. Metals. 2018. No. 8. p. 346. DOI: 10.3390/met8050346
16. Zhukov D., Konovalov S., Afanasyev A. Morphology and development dynamics of rolled steel products manufacturing defects during long-term operation in main gas pipelines. Engineering Failure Analysis. 2020. Vol. 109. DOI: 10.1016/j.engfailanal.2019.104359
17. Golikov I. N. Dendrite liquation in steel. M., Metallurgiya. 1958. 206 p.
18. Lesoult G. Macrosegregation in steel strands and ingots: characterization, formation and consequences. Mater. Sci. Eng. A. 2005. 413–414, pp. 19–29. DOI: 10.1016/j.msea.2005.08.203
19. Wu M., Könözsy L., Ludwig A., Schützenhöfer W., Tanzer R. On the formation of macrosegregations in steel ingot castings. Steel Res. Int. 2008. Vol. 79 (8). pp. 637–644. DOI: 10.1002/srin.200806177
20. GOST 19200-80. Iron and steel castings. Terms and definitions of defects. http://docs.cntd.ru/document/gost-19200-80 (access date 14.09.2020).
21. GOST 31447-2012. Steel welded pipes for trunk gas pipelines, oil pipelines and oil products pipelines. Specifications. http://docs.cntd.ru/document/1200103347 (access date 14.09.2020).
22. GOST R ISO 10893-9-2016. Seamless and welded steel tubes. Part 9. Automated ultrasonic testing for the detection of laminar imperfections in strip/plate used for the manufacture of welded steel tubes. http://docs.cntd.ru/document/1200133102 (access date 14.09.2020).
23. GOST R ISO 10893-8-2017. Seamless and welded steel tubes. Part 8. Automated ultrasonic method of testing for the detection of imperfections. http://docs.cntd.ru/document/1200157819 (access date 14.09.2020).
24. GOST 31447-2012. Steel welded pipes for main gas, oil and oil products pipelines. Technical conditions http://docs.cntd.ru/document/1200103347 (access date 27.02.2020).
25. GOST 1050-88. Graded and sized rolled metal with specially machined surface manufactured from quality constructional steel. General technical conditions (with revisions N 1, 2) http://docs.cntd.ru/document/1200004986 (access date 27.02.2020).
26. Failure analysis of heat treated steel components, ASM International, 2008, 640 p.
27. GOST R 54570-2011. Steel. Assessing the degree of banding or orientation of microstructures. http://docs.cntd.ru/document/1200093206 (access date 14.09.2020).

Полный текст статьи Metallography of non-metallic inclusions in pipe metal and impact assessment of defect structures on non-destructive testing outcomes
Назад