Название Features of tungsten extraction from spent catalysts of petroleum organic synthesis
DOI 10.17580/tsm.2017.11.06
Автор Pikulin K. V., Selivanov E. N., Galkova L. I., Gulyaeva R. I.
Информация об авторе

Institute of Metallurgy of Ural Branch of Russian Academy of Sciences, Ekaterinburg, Russia:

K. V. Pikulin, Junior Researcher, Post-Graduate Student, e-mail: pikulin.imet@gmail.com
E. N. Selivanov, Head of Laboratory, e-mail: pcmlab@mail.ru
L. I. Galkova, Researcher, e-mail: galkowa@mail.ru
R. I. Gulyaeva, Senior Researcher, e-mail: pcmlab@mail.ru

Реферат

We substantiated the treatment regimes for spent catalysts to obtain calcium tungstate. The technology, which allows to obtain calcium tungstate from low-quality raw materials, was taken as a basis. It provides for oxidative roasting, cinder sintering with soda, water leaching of sintered mass and precipitation of calcium tungstate from solution. The spent hydrotreating catalyst was taken as an initial sample. The composition of the catalyst is as follows, %: 13.7 W, 2.7 Ni, 28.2 Al, 7.8 S, 0.3 Si, 2.6 Fe and 20.0 C. According to X-ray phase analysis, the main phase of the catalyst is γ-Al2O3. Tungsten, nickel and iron are represented as oxides (WO3, NiO, Fe2O3), sulfides (WS2, NiS, FeS) and NiWO4 compounds. High content of carbon complicates the hydrometallurgical processing of catalyst. And high sulfur content does not allow its use for direct alloying of steel. Oxidative firing of the catalyst was used to reduce the carbon and sulfur contents. According to the data of thermal and X-ray diffraction (XRD) analyzes, the features of phase formation during oxidative roasting (900 оC) of spent catalysts were established. The process was accompanied by oxidation of carbon and sulfides and the formation of oxides of tungsten, nickel, iron and Al2(WO4)3. The formation of Al2(WO4)3 prevented the complete extraction of tungsten in the solution during leaching. The transfer of tungsten into a water-soluble form is possible by sintering the calcined catalyst with sodium carbonate at a temperature of 800 оC. According to the XRF data, the basis of the sintered mass was sodium tungstate. Oxides of  aluminum, iron and nickel were also identified. After aqueous (90–100 оC) leaching (l : s = 4), the oxides of aluminum, nickel and iron were concentrated in the cake. Calcium tungstate was precipitated from the solution by calcium nitrate at a pH of 10–12 and a temperature of 90–95 оC. It contained, %: 58.9 W, 13.9 Ca, 0.37 S. The extraction of tungsten in a commercial product was close to 90%.

Ключевые слова Spent catalyst, tungsten, aluminum oxide, nickel, sulfur, technology, thermal analysis, phase analysis, oxidizing roasting, sintering, leaching, calcium tungstate
Библиографический список

1. Tomina N. N., Pimerzina A. A., Moiseev I. K. Sulfide hydrotreating catalysts of petroleum feedstocks. Rossiyskiy khimicheskiy zhurnal. 2008. Vol. 52, No. 4. pp. 41–52.
2. Nazarov T. E., Dolmatov L. V. Hydrockracking catalysts development. Bashkirskiy khimicheskiy zhurnal. 2013. Vol. 20, No. 2. pp. 119–124.
3. Pavlov A. V., Rimoshevskiy V. S. Processing of spent molybdenum-bearing catalysts from petrochemical synthesis. Izvestiya vuzov. Chernaya metallurgiya. 2016. Vol. 59, No. 1. pp. 5–10.
4. Medvedev A. S., Malochkina N. V., Balgaeva F. Sh. Hydrometallurgical method of processing of spent petroleum refining catalysis. Nauchnaya sessiya MIFI-2007. Vol. 9. Moscow : MIFI, 2007. pp. 136, 137.
5. Hoda S. Ahmed, Mohammed F. Menoufy. New Trends in Hydroprocessing Spent Catalysts Utilization Petrochemicals. Rijeka, Croatia : In Tech, 2012. DOI: 10.5772/38595
6. Palant A. A., Bryukvin V. A., Petrova V. A. et al. Modern hydroeletrochemical technologies of complex processing of non-traditional types of raw materials. Resursy. Tekhnologii. Ekonomika. 2005. No. 10. pp. 2–9.
7. Akcil A., Veglio F., Ferella F., Okudan M. D., Tuncuk A. A review of metal recovery from spent petroleum catalysts and ash. Waste Management. 2015. Vol. 45. pp. 420–433.
8. Al-Sheeha H., Marafi M., Raghavan V., Rana M. S. Recycling and recovery routes for spent hydroprocessing catalyst waste. Industrial and Engineering Chemistry Research. 2013. Vol. 52. pp. 12794–12801.
9. Sahu K. K., Agrawal A., Mishra D. Hazardous waste to materials: Recovery of molybdenum and vanadium from acidic leach liquor of spent hydroprocessing catalyst using alamine 308. Journal of Environmental Management. 2013. Vol. 125. pp. 68–73.
10. Berrebi G., Dufresne P., Jacquier Y. Recycling of spent hydroprocessing catalysts: Eurecat technology. Resources, Conservation and Recycling. 1994. Vol. 10, No. 1/2. pp. 1–9.
11. Sitdikov F. G., Galkova L. I., Pikulin K. V., Selivanov E. N. Obtaining of calcium tungstate from low-quality concentrates. Proceedings of scientific and practical conference “Abishev readings-2016. Innovations in complex processing of mineral raw materials”. Almaty, 2016. pp. 548–553.
12. Pikulin K. V., Galkova L. I., Selivanov E. N., Sitdikov F. G. Extraction of tungsten from spent catalysis of petroleum organic synthesis. Proceedings of the congress “Fundamental investigations and applied developments of the processing and utilization of technogenic formations”. Ekaterinburg : UrO RAN, 2017. pp. 578–581.
13. Matthews S., Taliana F., James B. Heat treatment of plasma-sprayed Al2O3 and Al2O3 – WO3 coatings between 500 and 1000 оC. Surface and Coatings Technology. 2012. Vol. 212. pp. 109–118.
14. Nikolov I., Nikolov V., Peshev P. Regions of phase crystallization and new double tungstates in the system Na2O – Al2O3 – WO3. Journal of Alloys and Compounds. 2003. Vol. 351, No. 1/2. pp. 202–207.
15. Selivanov E. N., Frolova L. G., Sorokin A. A., Kuznetsov L. P. Distribution of elements-impurities during the electric smelting of secondary raw materials with ferronickel obtaining. Tsvetnaya metallurgiya. 1996. No. 11/12. pp. 25–27.

Language of full-text русский
Полный текст статьи Получить
Назад